AWS E310T1-1/4 Steel Flux-cored Welding Wire

Description:

E310T1-1/4 gas clipeum filum fluxum coredinum pro "omni positione" glutino destinatum et adhiberi potest cum 75% Ar / 25% CO2 vel 100% CO2 gas protegens.


Product Detail

Product Tags

E310T1-1/4 WIRE FLUX-CORED

DISTRIBUTIO
AWS 5.22 Classis E310T1-1/4 / ASME SFA A5.22 Classis E310T1-1/4
UNS W31031 A#9 F#6

DESCRIPTIO
E310T1-1/4 gas clipeum filum fluxum coredinum pro "omni positione" glutino destinatum et adhiberi potest cum 75% Ar / 25% CO2 vel 100% CO2 gas protegens.
Parametri glutino optimized sunt ut ne crepuit calidus.

APPLICATIONS
E310T1-1/4 saepissime ad metallorum basium conglobantium compositionum similium compositionum, quales sunt AISI 310 ferrei.
E310T1-1/4 ad chalybem coagmentationem carbonis ad immaculatam ferrum adhiberi potest.
E310T1-1/4 adhiberi possunt ad mixturas vel reficiendas capita alta mixtura et corrosio dejectiones repugnantes eiusdem compositionis generalis.
Minimum calor initus utere – suadeant 30,000 Joules/In Maximum.
Vitare concava pugillo grana
Serva interpass temperatus sub CCL°F
Imple omnia incipiunt et desine crateres ad rimas craterum vitandas.

TYPICA CHEMISTRIA (%)

C Cr Ni Mo Mn Si P S Cu
.10 25.9 20.4 .10 1.4 .82 .015 .005 .08

TYPICA MACHINA

DISTRAHENTES FORTITUDO 89,000 PSI
LONGINQUITAS in II " 38%
CALOR TREATMENT NULLUS

Nota: Mechanica proprietatibus ostensum est utens C% CO2

OPTIMUM TYPICA WELDING parametri (utendo C% CO2)

.045 DIA. CAMINUS & VERTIC Plana modo
AMPS 130-190 120-250
VOLTS 24-29 25-29
WFS (IPM) 225-450 200-600

NOTE: Exstare 3/8 "-1/2"
Volts inferior ab 2 cum usura 75% Ar / 25% CO2

Wenzhou Tianyu Electronic Co, Ltd. anno 2000 constitutum est. Nos in fabricandis electrodes conlocandis versati sumus,welding rodset glutino consumables plusquam XX annis.

Nostri principales fructus includunt chalybem immaculatum glutino electrodes, chalybeum glutinosum electrodes, stannum glutinosum electrodes, mixturas glutinosas electrodes, nickel & cobalt mixturas glutinosas electrodes, chalybem mitem & fila mixturae mixturae, intemerata chalybea glutino filis, filis coredis fluxus gas- clypei; filis aluminium glutino immersus arcu glutino.fila, nickel & cobalt filis mixturae glutino, filis glutinis aenei, filis glutinis TIG & MIG, electrodes tungsten, electrodes carbonis fodientes, et alia glutinosa accessiones & consumabiles.


  • Previous:
  • Deinde: