Inscriptio electronica:info@tyuelec.com Tel.:+86-577-62511131

Filum ad soldandum chalybem inoxidabilem AWS ER316LSi, virgae ad soldandum MIG et TIG, virgae ad implendum.

Descriptio Brevis:

Filum ad suturam chalybis inoxidabilis magnam efficaciam obductionis et bonam efficaciam technicam in sutura omnibus positionibus praebet. Late in industria adhibetur: in structuris aedificatoriis, vehiculis, pontibus, machinis fodinarum, ferriviis, tubis olei, apparatu pressionem gasi sustinente, apparatu potentiae, et cetera.


Detalia Producti

Etiquettae Productarum

Classificatio AWS: AWS 5.9

DESCRIPTIO:

Filum ad suturam chalybis inoxidabilis magnam efficientiam obductionis et bonam efficaciam technicam in sutura omnibus positionibus praebet. Late in industria adhibetur: in structuris aedificiorum, vehiculis, pontibus, machinis fodinarum, ferriviis, tubis olei, apparatu pressionem gasi sustinente, apparatu potentiae, et cetera.

NUMERUS MODELLI ET MAGNITUDO:

1. Officina suppleat officium OEM.

2. Exemplar: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi etc.

3. Magnitudo fili MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4. Magnitudo fili TIG: 1.6mm, 2.0mm, 2.4mm, 3.2mm, 4.0mm.

INTRODUCTIO:

Varias species filorum ad soldandum chalybem inoxidabilem praebemus, inter quas filum solidum ad soldandum Mig, filum ad soldandum virgas Tig, et filum ad soldandum arcu submerso, omnia summae qualitatis et toto orbe terrarum venduntur.

Praeter 308 et 309, etiam offerimus 304, 321, 347, 316L, 310, 2209, et 201. Necnon specificationes speciales ut 318L, 904L, 2594, NiCrMo-3, Ni1.

INVOLUCRUM:

Sarcinae filorum ad sudanda MIG (sarcinae tympani et sphaerae)

Diameter: 0.8 - 2.0mm

Sarcina: 1 kg/volumen, 5 kg/volumen, 15 kg/volumen, 20 kg/volumen, 100 kg/tympanum, 200 kg/tympanum

Sarcina filorum sudandi virgae TIG (tubus plasticus)

Diameter: 1.0 - 5.0mm

Sarcina: 5 kg/sarcina

Filum ad suduram arcus submersi

Diameter: 2.5 - 5.0mm

Sarcina: 20kg/sarcina, 25kg/sarcina

Involucra neutra et OEM grata sunt!

COMPOSITIONES CHEMICAE FILI SOLDANDI CHALYBIS INOXIDABILIS:

Numerus exemplaris

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

PROPRIETATES MECHANICAE FILI SOLDANDI:

Numerus exemplaris

Robur tensile Rm (Mpa)

Robur cedens Rel vel Rp0.2 (Mpa)

Elongatio

(%)

Numerus exemplaris

Robur tensile Rm (Mpa)

Robur cedens Rel vel Rp0.2 (Mpa)

Elongatio

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

Compositio fili ad sudandas TIG et MIG chalybem inoxidabilem

YB5092-2005

AWS

Compositio Chemica %

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1.80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Cu; 3 Nb; 0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N; 0.20 V; 0.18

Wenzhou Tianyu Electronic Co., Ltd. anno MM condita est. Plus quam XX annos in fabricatione electrodorum, virgarum soldandi, et rerum ad soldanda pertinentium versati sumus.

Inter producta nostra praecipua sunt electroda soldadurae chalybis inoxidabilis, electroda soldadurae chalybis carbonis, electroda soldadurae humilis mixturae, electroda soldadurae superficialis, electroda soldadurae niccoli et cobalti mixturae, fila soldadurae chalybis mollis et humilis mixturae, fila soldadurae chalybis inoxidabilis, fila nucleo fluxo protecta gaso, fila soldadurae aluminii, fila soldadurae arcus submersi, fila soldadurae niccoli et cobalti mixturae, fila soldadurae aeris, fila soldadurae TIG et MIG, electroda tungsteni, electroda excavationis carbonis, et alia accessiones et consumptibilia soldadurae.

 

Wenzhou Tianyu Electronic Co., Ltd. anno MM condita est. Plus quam XX annos in fabricatione electrodorum, virgarum soldandi, et rerum ad soldanda pertinentium versati sumus.

Inter producta nostra praecipua sunt electroda soldadurae chalybis inoxidabilis, electroda soldadurae chalybis carbonis, electroda soldadurae humilis mixturae, electroda soldadurae superficialis, electroda soldadurae niccoli et cobalti mixturae, fila soldadurae chalybis mollis et humilis mixturae, fila soldadurae chalybis inoxidabilis, fila nucleo fluxo protecta gaso, fila soldadurae aluminii, fila soldadurae arcus submersi, fila soldadurae niccoli et cobalti mixturae, fila soldadurae aeris, fila soldadurae TIG et MIG, electroda tungsteni, electroda excavationis carbonis, et alia accessiones et consumptibilia soldadurae.