Classificatio AWS: AWS 5.9
DESCRIPTIO:
Filum ad suturam chalybis inoxidabilis magnam efficientiam obductionis et bonam efficaciam technicam in sutura omnibus positionibus praebet. Late in industria adhibetur: in structuris aedificiorum, vehiculis, pontibus, machinis fodinarum, ferriviis, tubis olei, apparatu pressionem gasi sustinente, apparatu potentiae, et cetera.
NUMERUS MODELLI ET MAGNITUDO:
1. Officina suppleat officium OEM.
2. Exemplar: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi etc.
3. Magnitudo fili MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.
4. Magnitudo fili TIG: 1.6mm, 2.0mm, 2.4mm, 3.2mm, 4.0mm.
INTRODUCTIO:
Varias species filorum ad soldandum chalybem inoxidabilem praebemus, inter quas filum solidum ad soldandum Mig, filum ad soldandum virgas Tig, et filum ad soldandum arcu submerso, omnia summae qualitatis et toto orbe terrarum venduntur.
Praeter 308 et 309, etiam offerimus 304, 321, 347, 316L, 310, 2209, et 201. Necnon specificationes speciales ut 318L, 904L, 2594, NiCrMo-3, Ni1.
INVOLUCRUM:
Sarcinae filorum ad sudanda MIG (sarcinae tympani et sphaerae)
Diameter: 0.8 - 2.0mm
Sarcina: 1 kg/volumen, 5 kg/volumen, 15 kg/volumen, 20 kg/volumen, 100 kg/tympanum, 200 kg/tympanum
Sarcina filorum sudandi virgae TIG (tubus plasticus)
Diameter: 1.0 - 5.0mm
Sarcina: 5 kg/sarcina
Filum ad suduram arcus submersi
Diameter: 2.5 - 5.0mm
Sarcina: 20kg/sarcina, 25kg/sarcina
Involucra neutra et OEM grata sunt!
COMPOSITIONES CHEMICAE FILI SOLDANDI CHALYBIS INOXIDABILIS:
| Numerus exemplaris | C | Si | Mn | P | S | Cr | Ni | Mo | Cu |
| 304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
| 304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
| ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
| ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
| ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
| ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
| ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
| ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
| ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
| ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
| ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
| ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
| Numerus exemplaris | Robur tensile Rm (Mpa) | Robur cedens Rel vel Rp0.2 (Mpa) | Elongatio (%) | Numerus exemplaris | Robur tensile Rm (Mpa) | Robur cedens Rel vel Rp0.2 (Mpa) | Elongatio (%) |
| 304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
| 304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
| ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
| ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
| ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
| ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
| ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
| ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
| Compositio fili ad sudandas TIG et MIG chalybem inoxidabilem | ||||||||||
| YB5092-2005 | AWS | Compositio Chemica % | ||||||||
| C | Si | Mn | P | S | Cr | Ni | Mo | |||
| H08Cr20Ni9Mn7Si | ER307Si | 0.075 | 0.78 | 6.7 | 0.022 | 0.01 | 19.8 | 8.8 | ||
| H06Cr21Ni10 | ER308 | 0.045 | 0.45 | 1.9 | 0.02 | 0.009 | 20.8 | 9.8 | ||
| H0OCr21Ni10 | ER308L | 0.02 | 0.32 | 1.9 | 0.011 | 0.006 | 20 | 10.2 | ||
| H06Cr21Ni10Si | ER308Si | 0.045 | 0.85 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | ||
| H06Cr24Ni13 | ER309 | 0.06 | 0.45 | 1.9 | 0.019 | 0.009 | 24.3 | 13.2 | ||
| H06Cr24Ni13Si | ER309Si | 0.06 | 0.79 | 1.95 | 0.019 | 0.009 | 24.7 | 13.2 | ||
| H03Cr24Ni13 | ER309L | 0.02 | 0.42 | 1.8 | 0.02 | 0.01 | 24.8 | 13.2 | ||
| H03Cr24Ni13Si | ER309LSi | 0.018 | 0.8 | 1.7 | 0.02 | 0.01 | 23.5 | 13.5 | ||
| H21Cr16Ni35 | ER330 | 0.2 | 0.38 | 1.5 | 0.022 | 0.01 | 16.5 | 34.5 | ||
| H06Cr19Ni12Mo2 | ER316 | 0.04 | 0.4 | 1.9 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H06Cr19Ni12Mo2Si | ER316Si | 0.05 | 0.7 | 1.92 | 0.02 | 0.01 | 19.5 | 11.8 | 2.3 | |
| H03Cr19Ni12Mo2 | ER316L | 0.019 | 0.38 | 1.8 | 0.018 | 0.01 | 19.8 | 12.2 | 2.5 | |
| H03Cr19Ni12Mo2Si | ER316LSi | 0.06 | 0.85 | 1.7 | 0.022 | 0.01 | 18.8 | 12.6 | 2.4 | |
| H03Cr17Ni14Mo3 | ER317L | 0.02 | 0.38 | 1.8 | 0.02 | 0.01 | 18.8 | 13.8 | 3.6 | |
| H08Cr19Ni12Mo2Nb | ER318 | 0.06 | 0.42 | 1.5 | 0.022 | 0.01 | 18.5 | 11.8 | 2.3 | |
| H07Cr20Ni34Mo2Cu3Nb | ER320 | 0.06 | 0.4 | 1 | 0.022 | 0.01 | 19.8 | 33.3 | 2.8 | Nb0.7 |
| H02Cr20Ni34Mo2Cu3Nb | ER320L | 0.018 | 0.33 | 1.5 | 0.013 | 0.01 | 19.8 | 33.6 | 2.5 | Nb0.35 |
| H08Cr20Ni10Ti | ER321 | 0.06 | 0.45 | 1.5 | 0.022 | 0.01 | 20.8 | 9.8 | Ti9xC-1.0 | |
| H08Cr21 Ni10Nb | ER347 | 0.055 | 0.48 | 1.8 | 0.021 | 0.008 | 20.8 | 9.8 | Nb1xC-1.0 | |
| H12Cr26Ni21 | ER310 | 0.09 | 0.5 | 1.66 | 0.02 | 0.01 | 25.5 | 20.5 | ||
| H02Cr20Ni25Mo4Cu | ER385 | 0.02 | 0.3 | 1.5 | 0.018 | 0.01 | 20.2 | 24.8 | 4.8 | Cu 1.80 |
| H03Cr22Ni9Mo3N | ER2209 | 0.022 | 0.5 | 0.9 | 0.02 | 0.01 | 22.5 | 8.8 | 3.3 | N0.08-0.20 |
| H04Cr25Ni5Mo3Cu2N | ER2553 | 0.027 | 0.5 | 1 | 0.025 | 0.015 | 24.8 | 5.5 | 3.2 | N0.1-0.25 |
| H1 5Cr29Ni9 | ER312 | 0.09 | 0.38 | 1.5 | 0.022 | 0.01 | 29.5 | 8.5 | ||
| H03Cr24Ni13MoL | ER309L Mo | 0.023 | 0.45 | 1.5 | 0.022 | 0.01 | 23.8 | 13.2 | 2.2 | |
| H05Cr17Ni4Cu4Nb | ER630 | 0.04 | 0.39 | 0.5 | 0.022 | 0.01 | 16.5 | 4.8 | Cu; 3 Nb; 0.28 | |
| H08Cr26Ni5Mo2 | ER453s | 0.06 | 0.3 | 0.4 | 0.022 | 0.01 | 25.8 | 4.8 | 2.1 | |
| H08Cr21Ni10Mn6 | 0.06 | 0.35 | 5.5 | 0.022 | 0.01 | 20.8 | 9.8 | |||
| H05Cr22Ni11Mn6Mo3VN | ER209 | 0.04 | 0.4 | 4.5 | 0.022 | 0.01 | 21.5 | 10.8 | 2.2 | N; 0.20 V; 0.18 |
Wenzhou Tianyu Electronic Co., Ltd. anno MM condita est. Plus quam XX annos in fabricatione electrodorum, virgarum soldandi, et rerum ad soldanda pertinentium versati sumus.
Inter producta nostra praecipua sunt electroda soldadurae chalybis inoxidabilis, electroda soldadurae chalybis carbonis, electroda soldadurae humilis mixturae, electroda soldadurae superficialis, electroda soldadurae niccoli et cobalti mixturae, fila soldadurae chalybis mollis et humilis mixturae, fila soldadurae chalybis inoxidabilis, fila nucleo fluxo protecta gaso, fila soldadurae aluminii, fila soldadurae arcus submersi, fila soldadurae niccoli et cobalti mixturae, fila soldadurae aeris, fila soldadurae TIG et MIG, electroda tungsteni, electroda excavationis carbonis, et alia accessiones et consumptibilia soldadurae.
Wenzhou Tianyu Electronic Co., Ltd. anno MM condita est. Plus quam XX annos in fabricatione electrodorum, virgarum soldandi, et rerum ad soldanda pertinentium versati sumus.
Inter producta nostra praecipua sunt electroda soldadurae chalybis inoxidabilis, electroda soldadurae chalybis carbonis, electroda soldadurae humilis mixturae, electroda soldadurae superficialis, electroda soldadurae niccoli et cobalti mixturae, fila soldadurae chalybis mollis et humilis mixturae, fila soldadurae chalybis inoxidabilis, fila nucleo fluxo protecta gaso, fila soldadurae aluminii, fila soldadurae arcus submersi, fila soldadurae niccoli et cobalti mixturae, fila soldadurae aeris, fila soldadurae TIG et MIG, electroda tungsteni, electroda excavationis carbonis, et alia accessiones et consumptibilia soldadurae.