Soldatura Chalybis CarbonisElectrodum
J501Fe18
GB/T E5024
AWS A5.1 E7024
Descriptio: J501Fe18 est electrodum chalybis carbonis e pulvere ferreo, titanio similis, altae efficaciae. Efficacia depositionis est circa 180%, quae apta est ad soldaduram planam et soldaduram anguli plani.
Usus: Adhibetur ad soldaduram chalybis carbonis humilis, chalybis structuralis carinae generalis roboris Classis A, Classis B, et chalybis structuralis carinae altae roboris AH32, AH36.
Compositio chemica metalli conglutinati (%):
| C | Mn | Si | S | P |
| ≤0.12 | ≤1.25 | ≤0.60 | ≤0.035 | ≤0.035 |
Proprietates mechanicae metalli conglutinati:
| Res probata | Robur tensile MPA | Vis cedendi MPA | Elongatio % | Valor impetus (J) (0℃) |
| Garantitum | ≥490 | ≥400 | ≥23 | ≥47 |
Inspectio radiographica: gradus II
Currens commendatus:
| Diameter virgae (mm) | 3.2 | 4.0 | 5.0 | 5.6 | 6.0 |
| Currens soldandi (A) | 130 ~ 170 | CLXXX ~ CCXXX | 250 ~ 340 | 280 ~ 400 | 300 ~ 430 |
Wenzhou Tianyu Electronic Co., Ltd. anno MM condita est. Fabricationi operam dedimus...electrodum soldandis, virgas soldandi, et consumptibilia soldandi per plus quam viginti annos.
Inter producta nostra praecipua sunt electroda soldadurae chalybis inoxidabilis, electroda soldadurae chalybis carbonis, electroda soldadurae humilis mixturae, electroda soldadurae superficialis, electroda soldadurae niccoli et cobalti mixturae, fila soldadurae chalybis mollis et humilis mixturae, fila soldadurae chalybis inoxidabilis, fila nucleo fluxo protecta gaso, fila soldadurae aluminii, fila soldadurae arcus submersi, fila soldadurae niccoli et cobalti mixturae, fila soldadurae aeris, fila soldadurae TIG et MIG, electroda tungsteni, electroda excavationis carbonis, et alia accessiones et consumptibilia soldadurae.