AWS E8018-C1 Low Temperature Steel Welding Electrode W606Fe Low Hydrogen ARC Welding Rods

Description:

W606Fe (AWS E8018-C1) electrode ferri humilis est cum pulvere ferreo et infimo hydrogenii potassium efficiens


Product Detail

Product Tags

Humilis TemperatureSteel WeldingElectrode

W606Fe                                                     

GB/T E5518-C1

AWS A5.5 E8018-C1

Descriptio: W606Fe est humilis-temperatus ferrum electrodum cum pulvere ferreo et humile hydrogenium potassium efficiens.Adhiberi potest pro omni positione conglutinatio AC et DC.Depositum metallum bonam spissitudinem ictum in -60°C habet. 

Applicatio: Usus ad glutino temperaturae ferro humilis ut 2.5Ni.

 

Compositio chemica metallici solidi (%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

≤0.80

2.00 ~ 2.75

≤0.020

≤0.025

 

Mechanica metallorum congeries;

Test item

Distrahentes fortitudo

Mpa

Cedat imperium

Mpa

Prolongatio

%

Valorem impulsum (J)

-60℃

guaranteed

≥540

≥440

≥17

≥27

 

Diffusio hydrogenii contenti metalli depositi: ≤6.0mL/100g (modum glycerini) vel ≤10mL/100g (mercurius vel gasi methodo chromatographia)

X-ray inspection: I gradus

 

Commendatur current:

mm)

Rod diam

3.2

4.0

5.0

A)

Welding Current

90 ~ 120

140 ~ 180

180 ~ 210

 

Animadverte:

1. Electrodum coquendum est per 1 horae 350℃ ante operationem glutinum;

2. Essentiale est mundare ferruginem, squamam olei, aquam et immunditias in partibus glutino ante glutino.

 


  • Previous: