E70C-6M Carbon Steel Flux Cored Arc Welding Electrodes Flux Core Welding Wire

Description:

E70C-6M filum metalli-coredum glutino efficientiae solidi (GMAW) componit cum magnis fructibus rates fluvii-cored (FCAW) filis fumi generati-low rates, efficientiae altae, nulla scoria ad mundandum vel removendum-cum omnibus commodis cored. fila super fila solida habent - nullum "frigus gremium" vel fusione laterali carent, effectio pura cum 75-80% argonis / libra dioxydi carbonii, celeritas itineris celeritatis pro data vitta magnitudine.


Product Detail

Product Tags

E70C-6M filum metalli-coredum glutino efficientiae solidi (GMAW) componit cum magnis fructibus rates fluvii-cored (FCAW) filis fumi generati-low rates, efficientiae altae, nulla scoria ad mundandum vel removendum-cum omnibus commodis cored. fila super fila solida habent - nullum "frigus gremium" vel fusione laterali carent, effectio pura cum 75-80% argonis / libra dioxydi carbonii, celeritas itineris celeritatis pro data vitta magnitudine.E70C-6M applicationibus aptior est ubi gradus superiores manganesi et silicones essentiales sunt, quales sunt in praesentia scala molarum gravium vel levium contaminantium, vel auctus udus globuli globi desideratur.Productum hoc in communi proposito glutino excellit, sed aeque praestantior est in altioribus condicionibus postulantibus ac in graviore scheda metallica fabricatione, opere structurali, fistula glutino et coagmentatio aquarum calentium calidarum.

AWS Classis: E70C-6M Certification: AWS A5.18/A5.18M:2005
Admisce: E70C-6M ASME SFA A5.18

 

Wedding Position: F, H, V, OH .035-1/16"
F, H 5/64"-1/8"
Current:
DCEP

 

Fortitudo distrahens, kpsi; 70 100% CO2
Vires cede, kpsi; 58 100% CO2
Prolongatio in 2"%: 22 100% CO2

Typical Filum Chemiae sicut per AWS A5.18 (uno valores maxime)

C Mn Si S P Ni Cr Mo V Cu  
0.12 1.75 0.90 0.03 0.03 0.50 0.20 0.30 0.08 0.50  
Typical Welding Parametri
Diameter Processus Volt Amps protegens Gas
in (mm)
.035 (0.9) GMAW 24-35 160-250 75-95% Ar/balance Co2, 35-50cfh
.045 (1.2) GMAW 37-33 180-330 75-95% Ar/balance Co2, 35-50cfh
.052 (1.3) GMAW 25-35 220-460 75-95% Ar/balance Co2, 35-50cfh
1/16 (1.6) GMAW 26-37 240-520 75-95% Ar/balance Co2, 35-50cfh
5/64 (2) GMAW 27-36 240-550 75-95% Ar/balance Co2, 35-50cfh
3/32 (2.4) GMAW 28-36 350-550 75-95% Ar/balance Co2, 35-50cfh
7/64 (2.78 ) GMAW 27-34 400-600 75-95% Ar/balance Co2, 35-50cfh
1/8 (3.2) GMAW 26-32 95-145 75-95% Ar/balance Co2, 35-50cfh

 

Wenzhou Tianyu Electronic Co, Ltd. anno 2000 constitutum est. Nos in fabricandis electrodes conlocandis versati sumus,welding rodset glutino consumables plusquam XX annis.

Nostri principales fructus includunt chalybem immaculatum glutino electrodes, chalybeum glutinosum electrodes, stannum glutinosum electrodes, mixturas glutinosas electrodes, nickel & cobalt mixturas glutinosas electrodes, chalybem mitem & fila mixturae mixturae, intemerata chalybea glutino filis, filis coredis fluxus gas- clypei; filis aluminium glutino immersus arcu glutino.fila, nickel & cobalt filis mixturae glutino, filis glutinis aenei, filis glutinis TIG & MIG, electrodes tungsten, electrodes carbonis fodientes, et alia glutinosa accessiones & consumabiles.


  • Previous:
  • Deinde: