Stainless Steel Welding Electrodes AWS E308-15 Welding rods with Low Hydrogen Coating

Description:

A107 (AWS E308-15) est humilis carbonis Cr19Ni10 electrode immaculata cum sodium sodium-hydrogenium humilem.


Product Detail

Product Tags

Stainless Steel WeldingElectrode

A107                                        

GB/T E308-15

AWS E308-15

Descriptio: A107 electrode inactus est humilis carbonis Cr19Ni10 cum low-hydrogenis sodium membranae.Usus DCEP (electro positivo directo) et in omnibus positionibus conflari potest.Metallum depositum magnam habet proprietates mechanicas et resistentiam intergranulares corrosionis.

Applicatio: Usus ad glutino corrosioni-resistenti 06Cr19Ni10 structurae inactae chalybeae cuius operandi temperatura minor est quam 300°C.Potest etiam aliquos chalyros conglutinare cum paupere weldability (ut summus chromium chalybis) et superficies strata ferrea incorrupta superficiei superficies.

 

Compositio chemica metallici solidi (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Mechanica metallorum congeries;

Test item

 

Distrahentes fortitudo

Mpa

Prolongatio

%

guaranteed

≥550

≥35

 

Commendatur current:

Rod diam

mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

A)

25 ~ 50

50~ 80

80~ 110

110 ~ 160

160 ~ 200

 

Animadverte:

1. Electrodum coquendum est per 1 horae 250℃ ante operationem glutino;

2. Corrosio resistentiae et ferrite contenti metalli depositi determinantur duplici consensu copiarum et demandarum.

 

 

Wenzhou Tianyu Electronic Co., Ltd. in 2000. instituti sumuswelding electrodes, welding rods, etglutino consumablesplus quam XX annis.

Nostri principales fructus includunt chalybem immaculatum glutino electrodes, chalybeum glutinosum electrodes, stannum glutinosum electrodes, mixturas glutinosas electrodes, nickel & cobalt mixturas glutinosas electrodes, chalybem mitem & fila mixturae mixturae, intemerata chalybea glutino filis, filis coredis fluxus gas- clypei; filis aluminium glutino immersus arcu glutino.fila, nickel & cobalt filis mixturae glutino, filis glutinis aenei, filis glutinis TIG & MIG, electrodes tungsten, electrodes carbonis fodientes, et alia glutinosa accessiones & consumabiles.